OK 76.18是一款适用于焊接1.Cr-0.5Mo牌号抗蠕变钢的LMA焊条。该焊条可产生稳定的电弧,飞溅损失极少。OK 76.18可熔敷具有抗裂纹和抗气孔特性的焊缝金属。焊缝金属的结垢温度约为575°C。
熔敷数据
Fusion time per electrode at 90% I max |
kg weld metal/kg electrodes |
Number of electrodes/kg weld metal |
安培 |
熔敷率 |
电压 V |
直径 |
40 sec |
0.58 kg |
136.0 |
55-80 A |
0.70 kg/h |
22 V |
2.0 x 300 mm |
52 sec |
0.58 kg |
88.0 |
70-110 A |
0.80 kg/h |
24 V |
2.5 x 300 mm |
65 sec |
0.59 kg |
49.0 |
95-150 A |
1.10 kg/h |
25 V |
3.2 x 350 mm |
90 sec |
0.64 kg |
23.0 |
130-190 A |
1.70 kg/h |
27 V |
4.0 x 450 mm |
95 sec |
0.64 kg |
14.5 |
150-260 A |
2.70 kg/h |
28 V |
5.0 x 450 mm |